FAQ nameplate production process
Question: What should be using a diamond cutting tool in the production process nameplate pay attention to?
A: 1 tool clamping to be positive, smooth rotation of the workpiece clamping also positive, flat, tight, so as not to damage the tool.
2. Depth of cut to be small, about 0.1mm, to prevent damage due to eating too cutter knife.
3. To turn backward knife, after retracting stop.
Question: How to get twill cutting surface and grid?
A: To select the size and position of the workpiece positioned to get a good cutter ideal twill, thickness and knife sharp lines concerned. To get the lattice of the workpiece before and after going on the cutter each cutting once.
Question: When pressing Braille signs, inconsistent thickness, how high light cutting?
A: It should be added on a carbide cutter roughing tool cutting leveling at first, then the diamond cutting tool, which also protects the highlight tool is not damaged, hardness alloy tool also plays a balancing role when rotating cutter.
Question: How high light plate production fixed in the machine?
A: In order to combine solid, should be used in high-quality 500 # Nitto double-sided tape. Braille signage or squeeze out the back two legs fixed after perforation.
Question: Are high-gloss surface may Braille signage screen printing?
Answer: Yes. Such signs seen abroad, there is dry again in Braille printed transparent red ink, but also very beautiful.
Question: What highlights cutting new uses?
A: The use of different cutting tools and machine can process a bright line on the plate panel, the bright side and the bright hole. Vertical machine is also useful to make special tooling on the machine table, carving a variety of patterns and designs on the workpiece.
Epoxy signs manual
Epoxy signs of manual operation:
???????Epoxy plate manual operation is different from Epoxy plate machining (For more see "Epoxy signage Operating Procedures"), to distinguish between specific request from for comparison.
1, the first ready for all kinds of substrates, such as: nameplates, badges, medals, etc. into the oven preheating temperature requirement of 60 degrees, the purpose of the removal of surface moisture.
2, the substrate was placed flat dehumidified consistent level of console board waiting drip.
3. The amount, take a clean beaker, accurate measurement, the B component, a 2: 1 weight ratio of mixing evenly (must be mixed, otherwise there will be sticky and with the substrate surface delamination phenomena , the manufacturers of the products are the same to do this). (Note: the proportion of the manufacturers are not the same, as the case may be).
4, and then with a good mixture into a vacuum oven, open real pump, removing bubbles mix in a vacuum.
5, take in the clean needle, the needle after defoaming Shuijingjiao suction tube, then measure and drip evenly in the prepared substrate (ie: signs, trademarks, etc.) of the surface, the general crystal layer thickness 2mm, let the natural leveling can be (Note: The above process is controlled within 30 minutes, so as not to increase the liquid viscosity, resulting in inoperable).
6, the substrate 3-5 minutes after instillation Shuijingjiao observe glue surface without bubbles or dust particles, if any small bubbles, usable pin to pierce, found dead have not stream Shuijingjiao to place, with Extradition can pin.
7, pouring good signs, at room temperature 20 ℃ -30 ℃ cured 10-24 hours harden, becoming left the surface of the crystal plate.
8, in case of stickers, trademarks, etc., in itself is very thin, and the boundary is not obvious, when pouring, likely to cause Shuijingjiao spill to reach 2mm thickness will be difficult, so make Shuijingjiao grasp different situations, control viscosity, In the application process, you can put 1-2 hours in order to increase the viscosity, adapt thin Shuijingjiao casting.
9, making more than 2mm thick crystal glue signs, can be divided into secondary Epoxy, after the first dispensing, curing for 3-5 hours, then dropping layer.
10, Epoxy after cleaning, regardless of manual dispensing, or automated dispensing, after the completion of the machinery, equipment, containers are required to clean, because the Shuijingjiao hardened, insoluble in any solvent, therefore it must not harden before the machine , the containers are required to clean (Recommendation: Use acetone or ethanol)
July 10, 2024
Wyślij je do tym dostawcy
July 10, 2024
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.